Processing Properties Metric English Comments
Gel Time 0.6167 min

@Temperature 218 °C
0.6167 min

@Temperature 424 °F
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)
3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate..