Polymer Property : Gel Time = 18.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 16.0 - 18.0 min

@Temperature 100 °C
16.0 - 18.0 min

@Temperature 212 °F
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System
RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process.