Processing Properties Metric English Comments
Gel Time 35.0 - 45.0 min

@Temperature 80.0 °C
35.0 - 45.0 min

@Temperature 176 °F
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System
RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process.