Polymer Property : Drying Air Flow Rate = 9000 l/min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Air Flow Rate 9000 l/min

@Temperature 80.0 °C,
Time 80.0 sec
318 ft³/min (CFM)

@Temperature 176 °F,
Time 0.0222 hour
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant
TENFIL TF200 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti..
Drying Air Flow Rate 9000 l/min

@Temperature 50.0 °C,
Time 120 sec
318 ft³/min (CFM)

@Temperature 122 °F,
Time 0.0333 hour
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant
TENFIL TF200 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti..
Drying Air Flow Rate 9000 l/min

@Temperature 80.0 °C,
Time 80.0 sec
318 ft³/min (CFM)

@Temperature 176 °F,
Time 0.0222 hour
Guarniflon TENFIL TF 400 Polytetrafluoroethylene Thread Sealant
TENFIL TF400 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti..
Drying Air Flow Rate 9000 l/min

@Temperature 50.0 °C,
Time 120 sec
318 ft³/min (CFM)

@Temperature 122 °F,
Time 0.0333 hour
Guarniflon TENFIL TF 400 Polytetrafluoroethylene Thread Sealant
TENFIL TF400 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti..