Processing Properties | Metric | English | Comments |
---|---|---|---|
Extrusion Rate | 600 g/min | 600 g/min | |
P & P Technology MS-N Nickel Graphite Conductive Adhesive P & P Technology conductive nickel/graphite adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp.. |