Hold Pressure |
80.0 - 100 MPa |
11600 - 14500 psi |
|
Eurotec® Tecoform® PO30 GB30 NL HS POM, 30% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA30 GR50 BK002 XA40 PA6.6, 50% glass fiber reinforced, flame retardant, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR15 GR003 XA70 PA6.6, 15% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR30 NL HW PA6.6, 30% glass fiber reinforced, hydrolysis stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR30 NL RM PA6.6, 30% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 GR15 NL XA70 PA6, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 NL FY70 PA6, flame retardant - halogen free (RoHS compliant), natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NBX0 HF75 NL PA6, 75% heavy reinforced, improved flexibility, natural
Information provided by Eurotec® |
Hold Pressure |
60.0 - 100 MPa |
8700 - 14500 psi |
|
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Information provided by Eurotec® |
Hold Pressure |
60.0 - 100 MPa |
8700 - 14500 psi |
|
Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Information provided by Eurotec® |
Hold Pressure |
60.0 - 100 MPa |
8700 - 14500 psi |
|
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
80.0 - 100 MPa |
11600 - 14500 psi |
|
Eurotec® Tecoform® PO30 GB20 NL HS POM, 20% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 AR20 NL HS PA6.6, 20% aramid fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 CR10 BK111 PA6.6, 10% carbon fiber reinforced, black
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 NL IH PA6.6, impact modified, natural
Information provided by Eurotec® |
Hold Pressure |
60.0 - 100 MPa |
8700 - 14500 psi |
|
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
60.0 - 100 MPa |
8700 - 14500 psi |
|
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec® |
Hold Pressure |
60.0 - 100 MPa |
8700 - 14500 psi |
|
Eurotec® Tecopet® PT74 GR45 BK002 PR PET, 45% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 KG30 NL 0G PA6, 30% glass fiber/glass bead reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 KG30NL IX PA6, 30% glass fiber/glass bead reinforced, impact modified, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 MF20 GR003 FY70 PA6, 20% mineral filled, flame retardant - halogen free (RoHS compliant), grey RAL 7035
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural
Information provided by Eurotec® |