Polymer Property : Hold Pressure = 5000 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hold Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
Injection
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Hold Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
Injection
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Hold Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
Injection
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane
Features: Low Compression SetUse: Hydraulic Seals and Gaskets Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Hold Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
Injection
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Hold Pressure 34.5 - 68.9 MPa
5000 - 10000 psi
Injection
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol.