Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 9.99996 - 15.0 min @Temperature 121 °C |
0.166666 - 0.250 hour @Temperature 250 °F |
|
Master Bond Supreme 3HT-80 High Strength Epoxy Adhesive Cures at 80°C Description: Master Bond Supreme 3HT-80 is a one component, heat curing epoxy system featuring excellent physical strength properties and toughness with an eye-catching curing temperature of 170-175.. |