Processing Properties Metric English Comments
Cure Time 48.0 min

@Temperature 120 °C
0.800 hour

@Temperature 248 °F
Oven
Lord Adhesives Thermosetâ„¢ MD-130 Electrically Insulating Die-Attach Adhesive
Lord MD-130 is a microelectronic grade, die-attach adhesive system for use in applications where electrical conductivity is not required. This system offers long, room temperature stability, fast cu..