Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 100 min

@Temperature 21.0 °C
1.67 hour

@Temperature 69.8 °F
Tack Free without MEK
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating
Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres..