Polymer Property : Cure Time = 1.98 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time <= 1.98 min

@Temperature 150 °C
<= 0.0330 hour

@Temperature 302 °F
touch dry
Gwent Electronic Materials C2021031D2 Electrode Ink
Electrode Ink C2021031D2 is a Silver Palladium (85/15) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form..
Cure Time <= 1.98 min

@Temperature 150 °C
<= 0.0330 hour

@Temperature 302 °F
touch dry
Gwent Electronic Materials C2021031D3 Electrode Ink
Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form..