Polymer Property : Cure Time = 1260 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 1260 min

@Temperature 25.0 °C
21.0 hour

@Temperature 77.0 °F
Overcoat End
Chesterton MRS S4+ Metal Rebuilding System
An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 ..
Cure Time 1260 min

@Temperature 25.0 °C
21.0 hour

@Temperature 77.0 °F
Overcoat End
Chesterton ARC S4+ 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375..