Polymer Property : Cure Time = 13.0 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 780 min

@Temperature 25.0 °C
13.0 hour

@Temperature 77.0 °F
Full Load
Chesterton ARC 988 Composite
Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi..
Cure Time 780 min

@Temperature 32.0 °C
13.0 hour

@Temperature 89.6 °F
Light Load
Chesterton MRS S4+ Metal Rebuilding System
An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 ..
Cure Time 780 min

@Temperature 32.0 °C
13.0 hour

@Temperature 89.6 °F
Light Load
Chesterton ARC S4+ 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375..