Polymer Property : Cure Time = 18000 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 18000 min

@Temperature 16.0 °C
300 hour

@Temperature 60.8 °F
Full Chemical
Chesterton MRS S4+ Metal Rebuilding System
An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 ..
Cure Time 18000 min

@Temperature 16.0 °C
300 hour

@Temperature 60.8 °F
Full Chemical
Chesterton ARC S4+ 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375..