Processing Properties Metric English Comments
Cure Time 1140 min

@Temperature 16.0 °C
19.0 hour

@Temperature 60.8 °F
Light Load
Chesterton ARC 791 Composite
Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex..
Cure Time 1140 min

@Temperature 32.0 °C
19.0 hour

@Temperature 89.6 °F
Full Load
Chesterton ARC 791 Composite
Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex..