Processing Properties Metric English Comments
Cure Time 15.0 - 20.0 min

@Temperature 60.0 °C
0.250 - 0.333 hour

@Temperature 140 °F
Lord Adhesives Thermosetâ„¢ SC-102 Unfilled Silicone Encapsulant
Lord SC-102 is a "water-white" clear, two component, silicone encapsulating system. It has a very low viscosity and, when cured, a low Shore A hardness. Lord SC-102 is optically transparent with no ..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-301C Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-310G Bulk Compound
Appearance: Green silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by A..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-310R Bulk Compound
Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arl..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-322 Bulk Compound
Product Use: Silicone rubber (bulk compound)Appearance: Red silicone rubber.This data represents typical values for the production material. The data should not be used to write, or in place of, mat..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-338R Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-368 Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-390C Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-434R Bulk Compound
Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arl..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-493C Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-494 Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
Arlon CP-339R Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..