Polymer Property : Cure Time = 300 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 4320 - 18000 min

@Temperature 23.9 °C
72.0 - 300 hour

@Temperature 75.0 °F
Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating
Product Description: Master Bond EP21LVSP6 is a two component epoxy compound for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at room temperature or more ra..