Polymer Property : Cure Time = 30200 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 20200 - 30200 min

@Temperature 25.0 °C
336 - 504 hour

@Temperature 77.0 °F
Complete Cure Cycle
Northstar Polymers MPP-A80H Room-Temperature Curable Polyurethane
MPP-A80H has been specifically formulated to service applications where high elongation and good physical strength are required as well as where temperature during the process must be low for a very..