Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 27900 min @Temperature 10.0 °C |
465 hour @Temperature 50.0 °F |
Full Chemical |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |