Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 50.0 min @Temperature 60.0 °C |
0.833 hour @Temperature 140 °F |
|
Dow Corning HV 1540/20P BASE AND CLEAR CURING AGENT 32 Shore, very low viscosity, castable hydrophobic silicone rubber with high tear strength and low temperature cure.Information provided by Dow Corning |