Polymer Property : Sintering Temperature = 1620 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Sintering Temperature 1620 °C
2950 °F
Nabaltec GRANALOX® NM 9620 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1620 °C
2950 °F
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1620 °C

@Time 3600 sec
2950 °F

@Time 1.00 hour
Nabaltec GRANALOX® NM 9634 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1620 °C

@Time 7200 sec
2950 °F

@Time 2.00 hour
Nabaltec GRANALOX® NM 9916 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..