Polymer Property : Sintering Temperature = 1680 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Sintering Temperature 1580 - 1680 °C
2880 - 3060 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9634 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..