Processing Properties Metric English Comments
Sintering Temperature 1150 - 1250 °C
2100 - 2280 °F
Dwell time of 10-30 mins
Gwent Electronic Materials C2010309P3 Platinum Paste
This product has been designed as a platinum paste suitable for high temperature firing applications on to electro-ceramic substrates such as NTC. It is capable of withstanding repeated firing at h..