Processing Properties | Metric | English | Comments |
---|---|---|---|
Sintering Temperature | 1650 - 1750 °C | 3000 - 3180 °F | Interval (dense ceramic parts) |
Nabaltec GRANALOX® NM 9915 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |