Processing Properties Metric English Comments
Middle Barrel Temperature 179 - 185 °C
355 - 365 °F
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 179 - 185 °C
355 - 365 °F
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 179 - 185 °C
355 - 365 °F
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 179 - 185 °C
355 - 365 °F
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 179 - 185 °C
355 - 365 °F
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 168 - 185 °C
335 - 365 °F
Ravago Manufacturing Americas Hylac® FR134 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 165 - 185 °C
329 - 365 °F
Huntsman AVALON® 75 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a specially designed,..
Middle Barrel Temperature 165 - 185 °C
329 - 365 °F
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane
Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,..
Middle Barrel Temperature 165 - 185 °C
329 - 365 °F
Huntsman AVALON® 70 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a speci..
Middle Barrel Temperature 175 - 185 °C
347 - 365 °F
Extrusion
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester
Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext..
Middle Barrel Temperature 179 - 185 °C
355 - 365 °F
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 179 - 185 °C
355 - 365 °F
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 179 - 185 °C
355 - 365 °F
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.