Processing Properties Metric English Comments
Middle Barrel Temperature 188 - 202 °C
370 - 396 °F
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber..