Polymer Property : Middle Barrel Temperature = 279 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 246 - 279 °C
475 - 535 °F
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 263 - 279 °C
505 - 535 °F
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302..
Middle Barrel Temperature 263 - 279 °C
505 - 535 °F
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced
Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Middle Barrel Temperature 260 - 279 °C
500 - 534 °F
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 260 - 279 °C
500 - 534 °F
A. Schulman ComAlloy Hiloy® 284 PPO Alloy, Glass/Graphite Reinforced
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Graphite Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.