Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 177 - 204 °C | 350 - 400 °F | |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4180 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4180 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Middle Barrel Temperature | 188 - 204 °C | 370 - 400 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Middle Barrel Temperature | 177 - 204 °C | 350 - 400 °F | Injection Molding |
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s.. |
|||
Middle Barrel Temperature | 188 - 204 °C | 370 - 400 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s.. |
|||
Middle Barrel Temperature | 188 - 204 °C | 370 - 400 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 177 - 204 °C | 350 - 400 °F | Injection Molding |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 188 - 204 °C | 370 - 400 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |