Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 157 - 207 °C | 315 - 405 °F | |
Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound
(discontinued **) Low heat release aviation gradeApplications: Kydex IM90 is designed for injection molded parts each need to meet the highest flammability requirements of the FAA (FAR 25.853d) for vertical burn, rat.. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 196 - 207 °C | 385 - 405 °F | |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |