Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 254 - 271 °C | 489 - 520 °F | |
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Middle Barrel Temperature | 254 - 271 °C | 489 - 520 °F | |
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |