Processing Properties Metric English Comments
Middle Barrel Temperature 302 - 313 °C
575 - 595 °F
Polymer Resources PC-G30-TFE15 Polycarbonate, 30% Glass Reinforced, 15% PTFE
Polycarbonate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Middle Barrel Temperature 302 - 329 °C
575 - 625 °F
Star Plastics PC731 Molding Grade PC
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 302 - 329 °C
575 - 625 °F
Star Plastics PC733R Molding Grade PC
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 302 - 329 °C
575 - 625 °F
Star Plastics PCGF10 Molding Grade PC with 10% Glass
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 302 - 329 °C
575 - 625 °F
Star Plastics PCGF20 Molding Grade PC with 20% Glass
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 302 - 329 °C
575 - 625 °F
Star Plastics PCGF30 Molding Grade PC with 30% Glass
Information provided by Star Plastics, Inc.