Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika L-1003PA Heat resistance, creep resistance, and excellent lubricantInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika P-1001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Middle Barrel Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |