Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: EuropeProduct Applications: Thi.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 218W V15 PA66, 15% glass fiber, DRY Description: Polyamide 66, reinforced with 15% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: North AmericaProduct Applications: TECHNYL Â.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V3.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Ap.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber and modified for enhanced injection molding.Available in: Europe Product Applications: This material offers an excellent combination b.. |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Front Barrel Temperature | 280 °C | 536 °F | |
Beijing Chemical Industry KAIFA® M106N MPPO Resin High Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Front Barrel Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
LG Chemical LUXY KS G55 Amorphous PA6 Description: Injection Molding, Amorphous PA6, High Modulus, High Impact, Low WarpageApplication: Electric/Electronic Components (LCD Bracket)Information provided by LG Chemical |
|||
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F | |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |