Processing Properties Metric English Comments
Front Barrel Temperature 143 °C
289 °F
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica..
Front Barrel Temperature 143 °C
289 °F
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica..