Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 154 - 171 °C | 310 - 340 °F | |
RheTech Products E206-01 Linear Low Density Polyethylene, Black Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 154 - 188 °C | 309 - 370 °F | |
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE) Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar.. |