Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 204 - 216 °C | 399 - 421 °F | |
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE) Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Front Barrel Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4465 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4465 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4490 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP... |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC SunPro® SP 200 P3081 Polypropylene Copolymer SunPro® SP 200 P 3081 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM PP .. |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 2015 Polypropylene Impact Copolymer X-PRO PP 2015 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 2019 Polypropylene Impact Copolymer X-PRO PP 2019 is a high impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 2025 Polypropylene Impact Copolymer X-PRO PP 2025 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 2040 Polypropylene Copolymer X-PRO PP 2040 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Front Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |