Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 229 - 241 °C | 445 - 465 °F | |
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 229 - 241 °C | 445 - 465 °F | |
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 229 - 241 °C | 445 - 465 °F | |
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 229 °C | 444 °F | Injection |
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |