Front Barrel Temperature 252 - 274 °C
485 - 525 °F
PTS PCA-3013 High Flow PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 252 - 268 °C
485 - 515 °F
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced
Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex
Front Barrel Temperature 252 - 268 °C
485 - 515 °F
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced
Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi..