Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources NY66-FRG25 Flame Retardant Nylon 66, 25% Glass Reinforced Nylon 66, 25% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources NY66-IM1-G33-[color]-H Nylon 66, 33% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 33% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened Nylon 66, 33% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Mitsubishi Iupilon® S2000UR 9.5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Samyang Trirex® PC-3025IR 10 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Entec Hylex® P1010FR Polycarbonate Information provided by Ravago. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |