Processing Properties Metric English Comments
Front Barrel Temperature 299 - 318 °C
570 - 605 °F
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 299 - 318 °C
570 - 605 °F
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 299 - 318 °C
570 - 605 °F
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 299 - 318 °C
570 - 605 °F
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 299 - 327 °C
570 - 621 °F
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, ..