Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 160 °C | 320 °F | Blow Film |
DuPont Appeel® LSR11D704 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable s.. |
|||
Front Barrel Temperature | 160 - 177 °C | 320 - 350 °F | |
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Front Barrel Temperature | 160 °C | 320 °F | Blow Film |
DuPont Appeel® LSR20D751 Lidding Sealant Resin Appeel® LSR20D751 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu.. |
|||
Front Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
Front Barrel Temperature | 160 - 179 °C | 320 - 355 °F | |
RheTech Products E204-00 High Density Polyethylene, Natural Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |