Polymer Property : Front Barrel Temperature = 320 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 138 - 160 °C
280 - 320 °F
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE)
Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha..