Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 320 - 325 °C | 608 - 617 °F | Injection Molding |
LG Chemical LUCON CP510F PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b.. |
|||
Front Barrel Temperature | 320 - 325 °C | 608 - 617 °F | Injection Molding |
LG Chemical LUCON PN9008 PPS+MF+GF Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212.. |
|||
Front Barrel Temperature | 320 - 325 °C | 608 - 617 °F | Injection Molding |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |