Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 234 °C | 453 °F | Extrusion Coating |
DuPont Appeel® LSR11N704 Lidding Sealant Resin
(discontinued **) Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal.. |
|||
Front Barrel Temperature | 234 °C | 453 °F | Extrusion Coating |
DuPont Appeel® LSR11D704 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable s.. |
|||
Front Barrel Temperature | 234 °C | 453 °F | Extrusion Coating |
DuPont Appeel® LSR11D554 Lidding Sealant Resin Appeel® LSR11D554 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals to poly.. |
|||
Front Barrel Temperature | 234 °C | 453 °F | Extrusion Coating |
DuPont Appeel® LSR11D625 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D625 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals .. |