Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Front Barrel Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |
|||
Front Barrel Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |
|||
Front Barrel Temperature | 210 - 243 °C | 410 - 469 °F | |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |