Polymer Property : Injection Velocity = 203 mm/sec Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Velocity 50.8 - 203 mm/sec
2.00 - 8.00 in/sec
NatureWorks® Ingeo™ 3801X Injection Grade PLA
Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork..