Polymer Property : Injection Velocity = 75.0 mm/sec Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Velocity 50.0 - 75.0 mm/sec
1.97 - 2.95 in/sec
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber
A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.