Processing Properties | Metric | English | Comments |
---|---|---|---|
Cushion | 0.300 - 0.640 cm | 0.118 - 0.252 in | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture) Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Cushion | 0.300 - 0.640 cm | 0.118 - 0.252 in | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |