Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 149 - 160 °C | 300 - 320 °F | |
RheTech Products E206-01 Linear Low Density Polyethylene, Black Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 149 °C | 300 °F | |
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica.. |
|||
Nozzle Temperature | 149 °C | 300 °F | |
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica.. |
|||
Nozzle Temperature | 149 - 165 °C | 300 - 329 °F | |
Green Dot Terratek® Flex GDH-B1 Compostable Bioplastic Elastomer GDH-B1 is an elastomeric bioplastic with a diverse range of potential applications. It is a starch-based elastomer that is strong, durable and pliable with an exquisite soft touch. The bioplastic i.. |
|||
Nozzle Temperature | 149 - 205 °C | 300 - 401 °F | Average value: 198 °C Grade Count:8 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |