Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynalloy™ OBC8200-BT50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8200-BT50 is a translucent grade to be used in blow molding applications. New Product. Commercial specifications have not been established. - Excellent Colorability - Rubbery FeelPurge.. |
|||
Nozzle Temperature | 177 - 188 °C | 350 - 370 °F | |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |